Figure 1
From: Bandgap tuning of mixed organic cation utilizing chemical vapor deposition process

Photographs of MAxFA1−xPbI3 films with (a–e) 10 and (f–j) 400 sccm H2 flow rates with growth time increasing from 5 to 25 min.