Table 1 Hall measurement of Sb2Te3 samples with different thickness for carrier concentration and mobility.
Hall coefficient (cm3/C) | Carrier Concentration (cm−3) | Carrier Mobility (cm2V−1s−1) | |
---|---|---|---|
Thin platelets | 0.1583 | 3.9429 × 1019 | 113.583 |
Thick platelets | 0.28994 | 2.1529 × 1019 | 61.4198 |