Table 3 RL values of the obtained nanohybrids at the calculated matching thickness (dm) and the real thickness (d ) in terms of geometrical effect.
Sample | d/mm | RL/dB | fm/GHz | dm/mm |
---|---|---|---|---|
G400 | 1.5 | −18.9 | 17.8 | 1.4 |
2.0 | −20.3 | 14.2 | 1.7 | |
2.5 | −21.0 | 10.2 | 2.3 | |
G450 | 1.5 | −20.1 | 15.4 | 1.4 |
2.0 | −36.1 | 11.6 | 1.9 | |
2.5 | −18.6 | 8.6 | 2.4 | |
G500 | 1.5 | −18.4 | 14.0 | 1.4 |
2.0 | −35.3 | 11.0 | 1.8 | |
2.5 | −19.3 | 8.0 | 2.4 | |
G550 | 1.5 | −13.3 | 15.4 | 1.4 |
2.0 | −18.5 | 11.8 | 1.8 | |
2.5 | −32.1 | 8.8 | 2.4 |