Figure 4

Dependence of the atomic compositional depth profiles on a nanoscale spacer material for double MgO based p-MTJ spin-valves ex-situ annealed at 400 °C for 30 min under perpendicular applied field of 3 Tesla.
(a) Ta spacer of 0.4 nm and (b) W spacer of 0.4 nm.