Table 1 Comparison of solution-processed green phosphorescent PLEDs.

From: Bipolar and Unipolar Silylene-Diphenylene σ-π Conjugated Polymer Route for Highly Efficient Electrophosphorescence

Polymer host

EQE (%)

CEmax (cd/A)

PEmax (lm/W)

Von (V)

Ref.

This work Si(tOXD)(oTPA)a

21.2

80.1

62.9

4.0

Mixed host

 PVK:OP2a

13.6

44.6

5.9

9

 PVK: OXD-7b

110.7

29.3

12.0

10