Figure 3

Solidified microstructures of undercooled Ni83.25Zr16.75 peritectic alloy at undercooling of (a,b) ΔT = 9 K, (c) ΔT = 77 K, and (d) ΔT = 160 K.

Solidified microstructures of undercooled Ni83.25Zr16.75 peritectic alloy at undercooling of (a,b) ΔT = 9 K, (c) ΔT = 77 K, and (d) ΔT = 160 K.