Figure 8

From: Natural ageing responses of duplex structured Mg-Li based alloys

Figure 8

Observations to side surfaces near the fracture sites of: (a) and (c) Mg-6%Li alloy before and after natural ageing for 35 days, (e) and (g) Mg-6%Li-6%Zn-1.2%Y alloy before and after natural ageing for 35 days. Images (b,d,f and h) are high magnification observations to the squared areas in images (a,c,e and g), respectively.