Figure 8
From: Initiation and growth kinetics of solidification cracking during welding of steel

ADW test rig setup showing, (a) Side view of the design model in pre-test settings schematically illustrating key components, (b) ADW test rig embedded into ID19 beamline. The sample is in post-test deformed state and the yellow arrow dictates the approximate path of the X-ray through the 8 × 10−3 m thickness sample towards the detector.