Table 3 Thermal properties of nanocomposites.
From: Facile synthesis of high strength hot-water wood extract films with oxygen-barrier performance
Curve | Tonset (°C) | Tmax (°C) | Residuals (wt%) at 700 °C |
|---|---|---|---|
F1.5-1 | 181.3 | 218.2 | 80.5 |
F1-1 | 186.1 | 221.1 | 83.5 |
F1-1.5 | 188.4 | 224.8 | 84.4 |
FCMC0.05 | 188.2 | 223.9 | 82.4 |