Figure 4

(a) CV curves of the CF, CoMoO4 NWs, NiMoO4·xH2O NSs, and CoMoO4@NiMoO4·xH2O core-shell heterostructures at a scan rate of 5 mV s−1; (b) CV curves of CoMoO4@NiMoO4·xH2O at the scan rate between 5 and 100 mV s−1; (c) Charge and discharge curves of CoMoO4@NiMoO4·xH2O at different current densities ranged from 1 to 15A g−1; (d) Plots of the current density against specific capacitances of the CoMoO4 NWs, NiMoO4·xH2O NSs and CoMoO4@NiMoO4·xH2O core-shell heterostructures electrodes obtained from the galvanostatic charge-discharge curves; (e) Cycling performance of CoMoO4 NWs, NiMoO4·xH2O NSs and CoMoO4@NiMoO4·xH2O core-shell heterostructures at a discharge current density of 1A g−1; (f) Nyquist plots of CoMoO4 NWs, NiMoO4·xH2O NSs and CoMoO4@NiMoO4·xH2O core-shell heterostructures.