Figure 6 | Scientific Reports

Figure 6

From: Assembly of flexible CoMoO4@NiMoO4·xH2O and Fe2O3 electrodes for solid-state asymmetric supercapacitors

Figure 6

(a) CV curves of the CoMoO4@NiMoO4·xH2O//Fe2O3 ACS device coll ected at different potential voltages at a scan rate of 5 mV s−1; (b) CV curves of the CoMoO4@NiMoO4·xH2O//Fe2O3 ASC device collected at various scan rates; (c) Charge-discharge curves of the CoMoO4@NiMoO4·xH2O//Fe2O3 ASC device collected at various current densities; (d) Cycling performance of the CoMoO4@NiMoO4·xH2O//Fe2O3 ACS device at a discharge current density of 3A g−1 for 5000 cycles. The insets are charge-discharge curves of the CoMoO4@NiMoO4·xH2O//Fe2O3 ASC device collected at the first tenth and the last tenth cycles; (e) Charge-discharge curves of the CoMoO4@NiMoO4·xH2O//Fe2O3 ASC device collected at 3 Ag−1 under different bending conditions; (f) The Ragone plots relating power density to energy density of the supercapacitor devices and comparable previous studies.