Figure 6
From: Enhanced delignification of steam-pretreated poplar by a bacterial laccase

Synergy between sLac and Celluclast® 1.5 L during hydrolysis of the SPP. The data shows the extent of cellulose hydrolysis after 72 h using different dosages of protein (mg/g cellulose). Reactions were incubated in a rotary shaker for 72 h at 30 °C in 50 mM sodium acetate, pH 5. Reactions were performed in triplicate.