Table 2 Molar mass distribution of APPL recovered from steam pretreated poplar (SPP) with and without sLac.

From: Enhanced delignification of steam-pretreated poplar by a bacterial laccase

 

Molar mass distribution

Polydispersity (Mw/Mn)

Weight average (Mw)

Number average (Mn)

Peak 1

Peak 2

Peak 1

Peak 2

Peak 1

Peak 2

− sLac

11400 (300) a

5900 (200)

9629 (200)

4200 (100)

1.18 (0.04)

1.41 (0.05)

+ sLac

5070 (10)

3320 (10)

4680 (90)

3290 (10)

1.08 (0.04)

1.01 (0.01)

  1. aValue in parentheses indicates standard deviation.