Table 2 A comparison of the electrochemical effective area Aeff, calculated via the quasi-reversible Randles–Ševčík equation (see Methods section) and the geometrical surface area AGeo, (calculated from the physical contact area immersed within 1 mM hexaammineruthenium (III) chloride/0.1 M KCl) of the graphene/PLA and printed 3DE. The real area percentage, AReal, is also presented for additional comparison (see Methods section).
Electrode | AGeo/cm2 | Aeff/cm2 | AReal/% |
|---|---|---|---|
Graphene/PLA | 0.13 | 0.066 | 50.77 |
3DE | 0.36 | 0.085 | 23.61 |