Figure 6: The emission spectra of the precursor and GC fiber heat treated at 850 °C for 5 hours.
From: Glass-ceramic optical fiber containing Ba2TiSi2O8 nanocrystals for frequency conversion of lasers

The inset is the image of the GC fiber irradiated using the 1030 nm femtosecond laser.