Figure 4
From: Location, location & size: defects close to surfaces dominate fatigue crack initiation

SLS-17 specimen: (a) 3D rendering of the pores within the gauge. (b) 2D μCT reconstructed slice showing Pore 1′ state after 185,000 cycles. (c) Propagation stages of the internal crack nucleated at Pore 1′.