Figure 3
From: On the Role of the Electrical Field in Spark Plasma Sintering of UO2+x

Detail of the X-ray diffraction pattern of positive and negative surfaces of UO2 pellets sintered in SPS at 800 °C and 1000 °C for 5 minutes, starting from hyperstoichiometric powder.