The thiol-Michael polyaddition of three dialkynyl monomers with several dithiols proceeded using triethylamine as the catalyst to give unsaturated poly(ester-thioether)s with the expected structures (Mn, 2.4 × 103 to 22.6 × 103; molecular dispersity index [Mw/Mn], 1.26–2.00). All of the poly(ester-thioester)s had single glass-transition temperature values between −27 and 49 °C. While the rigid main chains improved the glass transition temperature, all of the poly(ester-thioester)s showed apparent enzymatic hydrolysis by lipase but low biodegradability in biodegradation tests using activated sludge.