Fig. 5: Electrochemical performance of TM6-ASSLBs. | Nature Communications

Fig. 5: Electrochemical performance of TM6-ASSLBs.

From: Maximizing interface stability in all-solid-state lithium batteries through entropy stabilization and fast kinetics

Fig. 5

a Charge/Discharge profiles of the all-solid-state battery at different rates from 25 mA/g to 100 mA/g. XRD patterns (b) and SEM/ EDS images of the HE-DRX-ASSLBs c before and d after cycling. e Cycling performance and f Coulombic efficiency of the HE-DRX-ASSLBs at 25 mA/g. All electrochemical measurements were performed at 150 °C without organic electrolyte and external pressure.