Fig. 3: Schematic of the heat evolved during DSC testing (heating cycles). | Nature Communications

Fig. 3: Schematic of the heat evolved during DSC testing (heating cycles).

From: Comprehensive analysis of ordering in CoCrNi and CrNi2 alloys

Fig. 3

Below around 748 K, the kinetics are too slow to change the CSRO in the experimental timescale. Above 748 K, CSRO can be either created (purple shade) or destroyed (red shade), as indicated by exothermic and endothermic reactions, respectively.

Back to article page