Fig. 5: The Application of NICL in Optoelectronic Devices.
From: Nanoimprint crystalithography for organic semiconductors

a Schematic of laser emission of the OMSB microdisk arrays fabricated by NICL. b The PL spectra of the OMSB microdisk at different pumping powers of 5.98, 19.02, 19.42, 22.07 μJ/cm2. c The emission intensity and FWHM as functions of the pumping power. d Schematic of OFET based on patterned OSCs fabricated by NICL. e Output curves of the OFET. f The transfer curve of the OFET. g Transfer curves of 6 × 6 OFET array based on patterned OSCs fabricated by NICL. h Mobility distribution in the 6 × 6 OFET array. i Corresponding histogram of saturation mobility. The average value is 3.15 cm2 V−1 s−1, and the standard deviation is 0.067 cm2 V−1 s−1.