Fig. 3: The yield stress with varying Al content.
From: Bayesian exploration of the composition space of CuZrAl metallic glasses for mechanical properties

The yield stress landscapes of Fig. 2 plotted as a function of the Al content for various fixed Cu/Zr ratios and for different cooling rates a \(\dot{T}=1{0}^{13}\) K/s, b \(\dot{T}=1{0}^{12}\) K/s, and c \(\dot{T}=1{0}^{11}\) K/s, showing a clear peak at cAl between 10% and 20% at low Zr concentrations.