Fig. 14: SEM (low and high magnification) images of artificially aged specimens of AA2024-T3 in UA condition (AA2024-T3+2h@190°C specimens).

Specimens’ fractured surfaces for: a 0.5 h, b 4 h and c 24 h of exposure to EXCO solution. after the tension test were examined through SEM microscope.