Fig. 12: The spontaneous elemental dissolution rates obtained from AESEC-OCP measurements, jsM (AESEC-OCP) compared with elemental dissolution rates extrapolated from AESEC-LSV curves at Ej=0, jM (AESEC-LSV). | npj Materials Degradation

Fig. 12: The spontaneous elemental dissolution rates obtained from AESEC-OCP measurements, jsM (AESEC-OCP) compared with elemental dissolution rates extrapolated from AESEC-LSV curves at Ej=0, jM (AESEC-LSV).

From: Element-resolved electrochemical database: AESEC polarization curves of ZnAlMg alloy coating constituents

Fig. 12

Data obtained from pure metals, intermetallic phases and commercial alloy coatings in 30 mM NaCl (pH = 8.4 and 10.1) as well as in 0.1 M NaOH (pH = 12.8) solutions are included. All repeated experimental data are also presented.