Fig. 7: XRD pattern of the corrosion product layer formed on LA2 coupons in seaport conditions (252 days of immersion).

A = aragonite, C = calcite, G = goethite, L = lepidocrocite, and M = magnetite. The diffraction lines are denoted with the corresponding Miller index (hkl).