Table 1 IM311/IGRS001 intensity ratio determined from XRD data of CS1, CS2 and LA1 steel grades
Steel grade | Cr content (wt.%) | IM311/IGRS001 Laboratory conditions | IM311/IGRS001 Seaport conditions |
|---|---|---|---|
CS1 | <0.05 | 0.54 | 0.43 |
CS2 | 0.15 | 1.56 | 0.28 |
LA1 | 0.8 | 5.96 | 0.81 |