Extended Data Fig. 3: Comparison of the degradation rates of the CCS and DCS-based PCECs under different steam concentrations with those of reported PCECs with the planar-contact electrode design. | Nature Energy

Extended Data Fig. 3: Comparison of the degradation rates of the CCS and DCS-based PCECs under different steam concentrations with those of reported PCECs with the planar-contact electrode design.

From: Conformally coated scaffold design using water-tolerant Pr1.8Ba0.2NiO4.1 for protonic ceramic electrochemical cells with 5,000-h electrolysis stability

Extended Data Fig. 3

BCMN/BZCYYb1711 (Ba2Co1.5Mo0.25Nb0.25O6−δ/BaZr0.1Ce0.7Y0.1Yb0.1O3−δ) (refs. 3,6,13,14,16,17,19,21,22,23,24,25,26,31,36,38,49,50,51).

Source data

Back to article page