Fig. 6: SHG and PL before and after the removal of MoS2 crystals on a low-density coated ECF.
From: In-fibre second-harmonic generation with embedded two-dimensional materials

a, SH power generated from 30 monolayers versus isolated monolayers on an identical ECF obtained by the ablation process. b, PL map from a typical MoS2 crystal before removal. The white dashed line displays the bottom of the exposed surface. c, PL map after the removal of the crystal in b using a pulsed laser at 515 nm. d, PL map from the retained crystal.