Table 2 Ranges of input printing conditions collected from the literature.

From: Laser powder bed fusion dataset for relative density prediction of commercial metallic alloys

Material

P (W)

v (mm/s)

h (mm)

l (mm)

s (mm)

References

316L

70-350

18.76–3400

0.018–0.16

0.02–0.46

0.035–0.2

14,17,34,35,36,37,38,39,40,41,42,43,44,45,46,47,48,49,50,51

IN718

90–400

100–2000

0.05–0.25

0.02–0.062

0.07–0.4

4,6,13,15,16,22,52,53,54,55,56,57

Ti6Al4V

35–400

40–3200

0.035–0.8

0.02–0.2

0.05–0.2

5,10,23,24,58,59,60,61,62,63,64,65,66,67

CuCrZr

160–600

100–1000

0.05–0.22

0.03–0.08

0.055–0.3

7,68,69,70,71,72,73,74,75,76,77

AlSi10Mg

100–950

100–10000

0.03–0.4

0.02–0.09

0.07–0.15

9,11,20,78,79,80,81,82,83,84,85,86,87,88,89

18Ni–300

50–450

200–3000

0.025–0.2

0.03–0.075

0.025–0.3

18,21,90,91,92,93,94,95,96,97,98,99,100