Table 5 Overpotentials at 200 mA·dm−2 and exchange current density of the obtained electrodes.
Electrodes | Foam Ni substrate | Foam NiZn + 600 °C | Foam NiZn + HCl |
---|---|---|---|
η200/mV | 582 | 360 | 306 |
j0/(A·cm−2) | 9.2 × 10−4 | 10.1 × 10−2 | 2.3 × 10−2 |
Electrodes | Foam Ni substrate | Foam NiZn + 600 °C | Foam NiZn + HCl |
---|---|---|---|
η200/mV | 582 | 360 | 306 |
j0/(A·cm−2) | 9.2 × 10−4 | 10.1 × 10−2 | 2.3 × 10−2 |