Table 2 Composition of different annealed BixIn35-xSe65 (x = 0, 5, 10 and 15) thin films.

From: Observation of high nonlinearity in Bi doped BixIn35-xSe65 thin films with annealing

Sample

Bi 0%

Bi 5%

Bi 10%

Bi 15%

Temp

 

350 °C

450 °C

 

350 °C

450 °C

 

350 °C

450 °C

 

350 °C

450 °C

Element

Cal (At.%)

Obs (At.%)

Obs (At.%)

Cal (At.%)

Obs (At.%)

Obs (At.%)

Cal (At.%

Obs (At.%)

Obs (At.%)

Cal (At.%)

Obs (At.%)

Obs (At.%)

In

35

34.52

34.61

30

29.35

29.39

25

24.29

24.24

20

19.39

19.46

Se

65

65.48

65.39

65

65.81

65.70

65

66.18

66.12

65

65.85

65.72

Bi

0

0

0

05

04.84

04.91

10

09.53

09.64

15

14.76

14.82

Total

100

100

100

100

100

100

100

100

100

100

100

100