Table 3 EIS parameters of carbon steel coupons in treated and control samples.

From: Sub-minimum inhibitory concentration of tetrakis(hydroxymethyl)phosphonium sulfate enhances biocorrosion of carbon steel by Pseudomonas aeruginosa

Treatment

Time (hr)

Rs (Ω cm2)

Yb−1 cm−2 sn)

nb

Rb (Ω cm2)

Ydl−1 cm−2 sn)

ndl

Rct (Ω.cm2)

Ceff (µf.cm-2)

Goodness of fit (χ2)

Control

24

6.70 ± 0.81

0.000342 ± 0.000048

0.8397 ± 0.0121

8.74 ± 1.61

0.000491 ± 0.000023

0.8977 ± 0.0261

1429 ± 108

255.8

0.0013

48

3.99 ± 0.33

0.000081 ± 0.000004

0.8496 ± 0.0161

24.78 ± 5.32

0.000265 ± 0.000037

0.9171 ± 0.0117

3350 ± 216

142.6

0.0017

72

13.85 ± 1.27

0.000261 ± 0.000021

0.8236 ± 0.0141

5.76 ± 0.9

0.000164 ± 0.000043

0.8683 ± 0.0109

5627 ± 301

65.1

0.0012

Treated (160 ppm THPS)

24

13.13 ± 1.52

0.000419 ± 0.000028

0.9641 ± 0.0203

4.90 ± 0.7

0.001233 ± 0.000116

0.8097 ± 0.0102

934 ± 62

466

0.0021

48

10.27 ± 0.77

0.000427 ± 0.000034

0.9721 ± 0.0186

8.66 ± 1.73

0.000623 ± 0.000218

0.8023 ± 0.0037

1238 ± 81

179.1

0.0015

72

12.80 ± 0.91

0.000413 ± 0.000128

0.9708 ± 0.0174

10.23 ± 1.89

0.000481 ± 0.000086

0.7952 ± 0.0104

5240 ± 254

129.6

0.0011