Table 3 Composition of prepared mixes with various CaO/SiO2 ratios.

From: Utilization of industrial waste materials for the preparation of wollastonite by temperature-induced forming technique

Powder (wt%)

CaO: SiO2 (wt ratio)

Silica fume (wt%)

Bypass (wt%)

PAA (wt%)

H2O (wt%)

65

1: 1

18.84

46.10

0.06

35.00

65

1: 1.17

20. 42

44.52

0.06

35.00

65

1: 1.25

21.62

43.32

0.06

35.00

65

1: 1.45

24.41

40.53

0.06

35.00