Table 6 EDX test of rock specimens before and after treatment with crude oil

From: Toward mechanistic understanding of wettability alteration in carbonate rocks in the presence of nanoparticles, gelatin biopolymer, and core-shell nanocomposite of Fe3O4@gelatin

EDX Analysis

O (w.%)

Ca (w.%)

C (w.%)

Br (w.%)

Si (w.%)

Fe (w.%)

Mg (w.%)

S (w.%)

Calcite rock before aging

52.45

30.96

12.99

1.41

1.19

1.01

Calcite rock aged with oil

1.72

11.23

83.45

0.25

3.36

Dolomite rock before aging

46.55

33.59

7.41

0.39

2.37

9.69

Dolomite rock aged with oil

31.13

11.79

49.18

7.09

0.81