Table 8 EDX test of rock specimens after treatment with SiO2 and Fe3O4 nanoparticles
EDX Analysis | O (w.%) | Ca (w.%) | C (w.%) | Si (w.%) | Mg (w.%) | S (w.%) | Cl (w.%) | Fe (w.%) |
---|---|---|---|---|---|---|---|---|
Calcite rock before aging | 1.72 | 11.23 | 83.45 | 0.25 | – | 3.36 | – | – |
Calcite rock aged by SiO2 nanofluid | 16.71 | 0.66 | 64.30 | 17.20 | – | 1.13 | – | – |
Dolomite rock before aging | 31.13 | 11.79 | 49.18 | – | 7.09 | 0.81 | – | – |
Dolomite rock aged by SiO2 nanofluid | 15.32 | – | 68.35 | 15.17 | – | 1.17 | – | – |
Calcite rock aged by Fe3O4 nanofluid | 6.09 | 2.04 | 54.03 | 0.33 | – | 1.81 | 3.52 | 32.18 |
Dolomite rock aged by Fe3O4 nanofluid | 16.07 | – | 50.06 | – | – | 1.53 | – | 32.35 |