Fig. 12

Variation in the conductivity vs. frequency for BNT-SrF5 bulk ceramics and thick film sintered for 15 min, at different temperatures from 205 to 310 °C.
Variation in the conductivity vs. frequency for BNT-SrF5 bulk ceramics and thick film sintered for 15 min, at different temperatures from 205 to 310 °C.