Table 1 Mass of the reagents used for the Preparation of SBF, and order in which they needed to be added to 1 L of deionised water.
From: Porous hydroxyapatite – β-tricalcium phosphate ceramics produced from a rapid sol-gel process
Order | Reagent | Amount (g) |
---|---|---|
1 | NaCl | 8.036 |
2 | NaHCO3 | 0.352 |
3 | KCl | 0.225 |
4 | K2HPO4 ⋅ 3H2O | 0.230 |
5 | MgCl2 ⋅ 6H2O | 0.311 |
6 | HCl | 40 mL |
7 | CaCl2 ⋅ 6H2O | 0.293 |
8 | Na2SO4 | 0.072 |
9 | Tris buffer | 6.063 |