Fig. 1 | Scientific Reports

Fig. 1

From: Development of a biodegradable α-TCP/PLA/nMgO composite for enhanced guided bone regeneration

Fig. 1

Mechanical properties of the composites with different PLA ratios. (A) SEM scanning of the outer surfaces and sections of different materials. Magnification: ×2000. (B) Flexural resistance of the materials. Significant to PLA: **P < 0.01, ***P < 0.001. Significant to others: ##P < 0.01, ###P < 0.001. (C) & (D) Vickers hardness of the materials. Significant to PLA: *P < 0.05, ***P < 0.001. Significant to others: ##P < 0.01.