Table 2 Mix calculations (kg/m3).

From: Microstructural evolution and mechanical property enhancement of red mud incorporated high strength concrete

Materials

B0RM

B5RM

B10RM

B15RM

B20RM

OPC

450

427.5

405

382.5

360

RM

0

22.5

45

67.5

90

Silica fume

85.4

85.4

85.4

85.4

85.4

Fine aggregates

589

589

589

589

589

Coarse aggregates

1180

1180

1180

1180

1180

Water

172

172

172

172

172

Super plasticizer

4.3

4.3

4.3

4.3

4.3