Fig. 9
From: Impact of propylene fibers and industrial wastewater on the properties of self-compacting concrete

28-day flexural (a) and tensile (b) strength results for different mixture designs of SCC.
From: Impact of propylene fibers and industrial wastewater on the properties of self-compacting concrete
28-day flexural (a) and tensile (b) strength results for different mixture designs of SCC.