Table 1 Spin coating parameters to fabricate 10 \(\upmu\)m thin PDMS membrane.
From: Mechanodynamic brain on chip for studying human stem cell derived neuronal networks
Steps | Acceleration (\(\text {rpm/s}^2\)) | RPM | Time |
|---|---|---|---|
1/3 | 250 | 2500 | 10 s |
2/3 | 0 | 2500 | 2.5 min |
3/3 | 250 | 0000 | 10 s |