Table 1 Summary of band edge positions and bandgap energies obtained using different methods of PEO and doped GO NPs at various concentrations.

From: Improved optical characteristics of PEO polymer integrated with graphene oxide

Sample

\(\:{\varvec{E}}_{\varvec{e}\varvec{d}\varvec{g}\varvec{e}}\:\mathbf{e}\mathbf{V}\)

\(\:{\varvec{E}}_{\varvec{o}\varvec{p}\varvec{t}}^{\varvec{d}}\) eV

\(\:{\varvec{E}}_{\varvec{o}\varvec{p}\varvec{t}}^{\varvec{i}\varvec{n}\varvec{d}}\) eV

\(\:{\varvec{E}}_{\varvec{i}\varvec{m}\varvec{a}\varvec{g}\varvec{i}\varvec{n}\varvec{a}\varvec{r}\varvec{y}}\) eV

PEO

5.77

5.82

5.56

5.86

PEOGO1

5.63

5.7

5.32

5.66

PEOGO3

3.00

3.33

2.78

2.69

PEOGO5

2.31

2.61

2.19

2.32

PEOGO7

2.27

2.51

2.12

2.22