Table 9 Analysis of variance (ANOVA) results for different surface properties.

From: Investigation of surface integrity in inconel 718 enhanced by heat treatment, ultrasonic impact and multi-media jet processing

 

Factor

Sum of Squares (SS)

Mean Square (MS)

F value

Significance

Surface roughness/µm

ATT/℃

2.062

0.687

33.6

Highly significant

USF/Hz

0.377

0.126

6.14

Significant

JP/MPa

0.181

0.060

2.95

Not significant

Surface microhardness/HV

ATT/℃

1349.2

4516.4

33.19

Highly significant

USF/Hz

606.9

202.3

1.49

Not significant

JP/MPa

1170.3

390.1

2.87

Not significant

Surface residual stress/MPa

ATT/℃

63769.7

21256.6

63.3

Highly significant

USF/Hz

1862.1

620.7

1.85

Not significant

JP/MPa

2000.3

666.8

1.99

Not significant