Table 2 Mean (standard deviation) of microtensile bond strength (MPa).

From: Effect of sulfinate salt on bonding and polymerization of adhesive to intracoronally bleached dentin

Groups

24 h

TC

Control

50.8 (5.8)Aa

50.8 (5.4)Aa

Bleached

34.7 (4.5)Ba

26.6 (7.1)Bb

Bleached + SA

50.6 (5.2)Aa

49.5 (8.8)Aa

  1. Significant differences in each column are indicated by the different superscript capital letters (p < 0.01). Significant differences in each row are indicated by the different superscript lowercase letter (p < 0.01). SA sulfinate agent, TC 10,000 thermal cycles.