Table 3 Compositions and gelation status obtained from bottle test and using Sydansk coding system.

From: Crosslinking a nanocomposite by zirconium sulfate to synthesize a high-durable new-generation polymer gel

Code

Polymer (wt%)

CL Con (wt%)

Time after gelation start (hrs)

1

2

4

6

8

10

12

24

1

0.5

0.1

A

B

B

C

D

E

E

G

2

0.5

0.3

B

D

D

E

E

F

F

H

3

0.5

0.5

C

D

D

E

F

F

F

F

4

0.5

1

C

C

C

E

E

E

E

E

5

0.75

0.1

C

D

D

E

F

F

G

H

6

0.75

0.3

B

C

D

D

D

E

E

H

7

0.75

0.5

B

B

B

D

E

E

F

G

8

0.75

1

B

B

C

C

D

E

E

F

9

1

0.1

C

D

E

E

E

F

G

H

10

1

0.3

B

D

E

F

G

G

H

H

11

1

0.5

A

B

D

F

F

G

G

H

12

1

1

A

B

C

D

F

F

G

G

13

1.25

0.1

C

C

D

E

F

G

H

H

14

1.25

0.3

D

E

F

F

G

G

H

H

15

1.25

0.5

D

F

F

F

G

G

G

H

16

1.25

1

C

C

C

D

F

F

F

G

17

1.5

0.1

D

D

E

F

G

G

H

H

18

1.5

0.3

D

E

F

F

G

H

H

H

19

1.5

0.5

D

E

E

F

F

G

H

H

20

1.5

1

B

C

D

E

E

F

G

H

21

2

0.1

D

E

G

G

H

H

H

H

22

2

0.3

D

E

G

H

H

H

H

H

23

2

0.5

C

D

E

G

G

H

H

H

24

2

1

C

D

E

F

F

G

H

H