Fig. 8

SEM backscattered electron images of Lu2SiO5 after interaction with molten CMAS at 1300 °C for 5 h. (a) Cross-section SEM image, (b) Higher resolution cross-section SEM image, (c) EDS elemental maps corresponding to the rectangular area in (b).