Fig. 6
From: Tensile plasticity in Cu and Ni-coated Ni54Nb42Al4 metallic glassy fibers

Five stages tensile déformation behavoir of bilayer Cu/Ni-coated Ni54Nb42Al4 MG fiber with different R values (a) Shows five stages deformation behavio of bilayer Cu/Ni-coated MG wire with R = 75% and (b) shows five stages deformation behavior of Cu/Ni-coated wire with R = 85% and clearly show a significance enhancement in tensile plasticity of thick coated MG wire.