Fig. 10

(a) Ac conductivity (σac) versus frequency for Cd0.40Mn0.60ZnO2 annealed nanocomposite samples (b) The linear plot of ln σac versus ln ω for Cd0.40Mn0.60ZnO2 annealed nanocomposite samples.