Table 2 The energy gap (Eg), residual dielectric constant (εL), carrier density (N/m*), photocatlytic efficiency and degradation rate of Cd0.40Ni0.60ZnO2 annealed nanocomposite samples.

From: Comprehensive study of optical, photocatalytic and dielectric properties of Cd0.40Mn0.60ZnO2 annealed nanocomposites

Tann

(oC)

Eg ±0.025

(eV)

εL

(N/m*)\(\:\times\:\)1054

(cm3.g)-1

Eo

(eV)

Ed

(eV)

(\(\:\varvec{\upeta\:}\:\))max

(%)

(150 min)

K

(s-1)

200

1.80

3.07

7.38

4.57

12.43

71.40

1X 10-5

300

1.75

2.24

8.61

3.17

6.68

74.28

1X 10-5

400

1.55

2.44

0.86

10.15

15.40

81.15

2X 10-4

500

1.95

3.22

0.74

10.58

23.33

62.08

7X 10-5

600

2.05

1.82

0.84

6.93

6.53

60.53

6X 10-5