Table 3 s, Wm and RPs of Cd0.40Mn0.60ZnO2 annealed nanocomposite samples.

From: Comprehensive study of optical, photocatalytic and dielectric properties of Cd0.40Mn0.60ZnO2 annealed nanocomposites

Tann

(oC)

s

Wm

(eV)

RPs (tanδ)

(KHz)

RPs (M\\)

(KHz)

RPs (Z\\)

(KHz)

tm (tanδ)

(µs)

tm (M\\)

(µs)

tm (Z\\)

(µs)

200

0.39

0.255

non

15

3.89

non

10.62

40.94

300

0.38

0.250

75.91

232

5.64

82.71

0.69

28.23

400

0.37

0.247

non

15

3.89

non

10.62

40.94

500

0.35

0.239

non

15

4.76

non

10.62

33.45

600

0.36

0.243

non

24.90

10

non

6.40

15.92